Grade | C | Si | Mn | P | S | Ni+Co | Cu | Fe |
Nickel 200 | <0.15 | <0.35 | <0.35 | <0.01 | >99.0 | <0.25 | <0.40 |
Grade | Density (g/cm3) | Melting Range (C) | Curie point (C) | Volume resistivity (μ.cm) | Thermal conductivity (W/m. C) |
Nickel 200 | 8.89 | 1435-1446 | 360 | 8.5(20C) | 79.3(20C) |
FORM |
Yield Strength(Mpa) |
Tensile Strength(Mpa) |
Elongation (%) |
Hardness(RB) |
|
Bar |
Hot-finished | 105-310 | 60-85 | 55-35 | 45-80 |
Cold-drawn, annealed | 105-210 | 55-75 | 55-40 | 75-98 | |
Strip |
Hard | 480-795 | 620-895 | 15-2 | >90 |
Annealed | 105-210 | 380-580 | 55-40 | <70 | |
Wire |
Annealed | 105-345 | 380-580 | 50-30 | |
No.1 Temper | 275-520 | 485-655 | 40-20 | ||
Spring Temper | 725-930 | 860-1000 | 15-2 |