Gluconic Acid Sodium Salt/Sodium Gluconate with retarding agent
OverviewQuick DetailsPlace of Origin:Shandong, China (Mainland)Brand Name:YU LAModel Number:YL-SGAppearance:White crystal PowderPurity:98%Ap
$5 /Ton
Stock: 300000 Tons
Quantity:
-+
Min Order: piece
Buy Now
Add To Cart
Send Inquiry
Seller Support:
Trade Assurance — To protect your orders from payment to delivery
Product Details
Transaction Comments
Overview
Quick Details
Place of Origin:
Shandong, China (Mainland)
Brand Name:
YU LA
Model Number:
YL-SG
Appearance:
White crystal Powder
Purity:
98%
Application:
tech & food
Type:
Set Retarder
Chloride content:
≤0.07
PH Value:
6.2-7.8
Packaging & Delivery
Packaging Details
For powder: 25kg woven plastic bag with film liner/ paper 650kg jumbo bag.
Delivery Time
Shipped in 7 days after payment
Product Description

 

YL-SG referred to as retarder, it is a set-retarding admixture, and it can slow down the hydration of cement, prolong set time, and extend the working life of concrete for long periods without any negative influence on the concrete quality. It complies with ASTM C494, Type B, GB8076-2008 and GB50119-2003.

Usage

 

YL-SG is beneficially used in hot weather conditions in order to overcome accelerating effects

 of higher temperatures. It can be widely applied in large masses of concrete. Freshly batched concrete for long hauls, shot concrete, and cast concrete.

 

Advantages

 

  • Extending concrete initial setting time for proper finishing without cold joint during hot weather.
  • Increasing the workable time of concrete up to several hours.
  • Providing flexibility in planning and scheduling of concrete pours.
  • Applicable for massive concrete, cast concrete and large area construction.

 

Dosage

 

0.01% to 0.06% by weight of cement. Exact dosage rates are dependent on the type of effect sought, quality of cement and aggregates, water/cement ratio and ambient temperature, Therefore, in many cAses it is advisable for carry out trial mixes.

 

Specification

 

Item

Specification

Visual Appearance

White or yellowish crystal powder

Loss on drying (%)

0.5 Max

Purity (%)

≥98

Reducing Substances (%)

≤0.7

Heavy metal (Pb), ug/g

≤10

Sulfate,%

≤0.05

Chloride,%

≤0.07

Lead, ug/g

≤2

Arsenic, ug/g

≤2

PH Value

6.2-7.8

 

Test Data Sheet

 

Items

Criteria

Test Results 

Ratio of Bleeding Rate (%)

≤100

49.1

Setting Time Difference (min)

Initial

>+90

+340

Compressive Strength Ratio (%)

3 days

≥100

135

7 days

≥100

130

28 days

≥100

123

Shrinkage (%

28 days

≤135

112

Alkali Content (%)

-----

2.50

Alkali Content per m3 (kg)

≤1.0

0

Chloride Ion Content

-----

0.40

Chloride Ion Content per m3(kg)

Prestress Concrete

<0.02

0.002

Reinforced Concrete

0.02~0.20

Plain Concrete

0.20~0.60

Ammonia Content (%)

≤0.1

0.01

Radiation

Internal Exposure Index,  IRa

≤1.0

0.28

External Exposure , Index,  IY

≤1.0

0.46

 

Packaging & Shipping

 

 

For powder: Woven plastic bag with film liner. Net weight: 25kg +/- 0.2 kg.

 

It should be stored in a dedicated warehouse that is well-ventilated and dry and keep away from moisture.

 

Shelf Life: Minimum 12 months. After the expiration date, it can be used if testing results is qualified.

Contact Us

 Gluco<em></em>nic Acid Sodium Salt/Sodium Gluco<em></em>nate with retarding agent

Other products from this supplier
Back to top
X
Added successfully
You have added this product to the wish list successfully !
X
Added successfully
It has now been moved to the top of the list!
Continue shopping
X
Add a New List
Save
cancel