Test Item | Unit | Standard | Test Method | |
Thickness Tolerance | % | ±5 | ASTM D-374 | |
Tensile strength |
MD | mpa | ≥200 | ASTM D-882 |
TD | ≥200 | |||
Elongation at break |
MD | % | ≥100 | ASTM D-882 |
TD | ≥100 | |||
Heat shrinkage (150ºC,30min) |
MD | % | ≤3.0 | ASTM D-1204 |
TD | ≤3.0 | |||
Surface Tension | mN/m | ≥52 | ASTM D-2578 | |
Friction Coefficient |
-- | ≤0.80 | ASTM D-1894 | |
≤0.80 | ||||
Base Film Haze | % | ≤3.0 | ASTM D-1003 | |
Thickness of Aluminum Layer |
Å | 380 | Square resistance meter | |
Ω/ | 1.50 | GB/T 15717 | ||
O.D | 1.80 | X-rite 361 | ||
Uniformity of Aluminum Layer |
% | ±10 | GB/T 15717 | |
Firm of Aluminum Layer |
% | 0 | 3M Tape |